SciEPublish

Stretchable Copper Micropatterns Embedded in Polydimethylsiloxane for Soft Wearable Devices

Article Open Access

Stretchable Copper Micropatterns Embedded in Polydimethylsiloxane for Soft Wearable Devices

Author Information
1
Department of Mechanical Engineering, Indian Institute of Technology Jammu, Jammu 181221, India
2
Department of Computer Science and Engineering, Indian Institute of Technology Jammu, Jammu 181221, India
*
Authors to whom correspondence should be addressed.

Received: 23 July 2026 Revised: 07 August 2026 Accepted: 06 November 2026 Published: 24 November 2026

Creative Commons

© 2026 The authors. This is an open access article under the Creative Commons Attribution 4.0 International License (https://creativecommons.org/licenses/by/4.0/).

Views:268
Downloads:56
Intell. Sustain. Manuf. 2026, 3(2), 10031; DOI: 10.70322/ism.2026.10031
ABSTRACT: Wearable devices worn directly on the body, for monitoring human motion, sensing as soft robotic skin, and health diagnostics, need conductive traces that stay connected and keep the signal stable when they are stretched or bent. First, micrometer-scale metal traces are hard to pattern on a soft substrate because conventional tools are designed for rigid wafers, and the substrate deforms during processing. Secondly, to address this, we patterned 36 μm copper foil laminated on the biocompatible elastomer polydimethylsiloxane (PDMS) by ultraviolet (UV) photolithography, using a dry film negative photoresist and maskless exposure at 365 nm. The exposure dose, the sodium carbonate developer concentration, and the ferric chloride etchant concentration were adjusted for each feature width, and the horseshoe-shaped traces were embedded by casting a second PDMS layer. Thirdly, qualitatively, a finite-element model showed that the adhesive under a 250 μm trace stays in compression up to 30% strain, whereas under a 1 mm trace it is pulled open, and that embedding reduces the out-of-plane deflection of the copper about fourfold. Furthermore, quantitatively, the process gave copper interconnects with a minimum linewidth of 250 μm and a thickness of 36 μm, and in a cyclic stretching test the embedded horseshoe interconnects kept the baseline of a strain sensor stable (a 7% relaxation, then a slow drift of about +0.02% per cycle, against +25% with straight copper leads) and made its response more linear and less hysteretic. Finally, the route needs no vacuum deposition, transfer step, or cleanroom.
Keywords: Photolithography; Stretchable substrate; Microfabrication of copper interconnects; Dry film negative photoresist; Etching; Stretchable electronics